Eliminating Bubbles on Polyamide Strips

Adapta Color S.L.

img

During the process of curing powder coatings on aluminium sections, bubbles frequently occur on the polyamide insulating strips and these are caused by water vapour in the polyamide. A new range of powder coatings significantly reduces the impact of this problem. 